Evaluation of the marginal and internal gap of metal-ceramic crown fabricated with a selective laser sintering technology: two- and three-dimensional replica techniques

Authors
Kim, Ki-BaekKim, Jae-HongKim, Woong-ChulKim, Hae-YoungKim, Ji-Hwan
Issue Date
5월-2013
Publisher
KOREAN ACAD PROSTHODONTICS
Keywords
CAD-CAM; Marginal adaptation; Metal ceramics restorations; Replica techniques
Citation
JOURNAL OF ADVANCED PROSTHODONTICS, v.5, no.2, pp.179 - 186
Indexed
SCIE
SCOPUS
KCI
Journal Title
JOURNAL OF ADVANCED PROSTHODONTICS
Volume
5
Number
2
Start Page
179
End Page
186
URI
https://scholar.korea.ac.kr/handle/2021.sw.korea/103283
DOI
10.4047/jap.2013.5.2.179
ISSN
2005-7806
Abstract
PURPOSE. One of the most important factors in evaluating the quality of fixed dental prostheses (FDPs) is their gap. The purpose of this study was to compare the marginal and internal gap of two different metal-ceramic crowns, casting and selective laser sintering (SLS), before and after porcelain firing. Furthermore, this study evaluated whether metal-ceramic crowns made using the SLS have the same clinical acceptability as crowns made by the traditional casting. MATERIALS AND METHODS. The 10 study models were produced using stone. The 20 specimens were produced using the casting and the SLS methods; 10 samples were made in each group. After the core gap measurements, 10 metal-ceramic crowns in each group were finished using the conventional technique of firing porcelain. The gap of the metal-ceramic crowns was measured. The marginal and internal gaps were measured by two-dimensional and three-dimensional replica techniques, respectively. The Wilcoxon signed-rank test, the Wilcoxon rank-sum test and nonparametric ANCOVA were used for statistical analysis (alpha=.05). RESULTS. In both groups, the gap increased after completion of the metal-ceramic crown compared to the core. In all measured areas, the gap of the metal cores and metal-ceramic crowns produced by the SLS was greater than that of the metal cores and metal-ceramic crowns produced using the casting. Statistically significant differences were found between cast and SLS (metal cores and metal-ceramic crown). CONCLUSION. Although the gap of the FDPs produced by the SLS was greater than that of the FDPs produced by the conventional casting in all measured areas, none exceeded the clinically acceptable range.
Files in This Item
There are no files associated with this item.
Appears in
Collections
College of Health Sciences > Division of Health Policy and Management > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Kim, Hae Young photo

Kim, Hae Young
보건과학대학 (보건정책관리학부)
Read more

Altmetrics

Total Views & Downloads

BROWSE