베릴륨이 포함되지 않은 도재용착주조관용 비 귀금속 합금의 재사용에 따른 금속과 도재간의 전단결합강도에 관한 연구
DC Field | Value | Language |
---|---|---|
dc.contributor.author | 김소리 | - |
dc.contributor.author | 김웅철 | - |
dc.contributor.author | 김혜영 | - |
dc.contributor.author | 김지환 | - |
dc.date.accessioned | 2021-09-06T07:36:38Z | - |
dc.date.available | 2021-09-06T07:36:38Z | - |
dc.date.created | 2021-06-17 | - |
dc.date.issued | 2013 | - |
dc.identifier.issn | 1229-3954 | - |
dc.identifier.uri | https://scholar.korea.ac.kr/handle/2021.sw.korea/105068 | - |
dc.description.abstract | Purpose: This study aimed to investigate the shear bond strength for non-precious alloy castings without beryllium, which has been used repeatedly for economical reason. Methods: The Schmitz-Schulmeyer test method was used to evaluate the shear bond strength between the nonberyllium Ni-Cr alloy Vera Bond 2V(AlbaDent, Inc. USA) and the Ceramco 3(Dentstply, York, PA, USA) porcelain powder. The maximum loading and shear bond strength were measured. The average shear strength( ) was analyzed with the one-way ANOVA and the Tukey’s test( =.05). The fracture specimens were examined using Microscope to determine the failure pattern. Results: The mean shear bond strengths(SD) in MPa were group A(100% new metal) control 28.72(3.31); group B(50% new + 50% reused) 27.28(1.13); group C(all reused) 26.61(5.47). Microscope examination showed that group A and B specimens presented mixed failure, and group C specimens showed adhesive failure. Conclusion: In conclusion, forward this non-precious alloy dose not contain beryllium for how should use a more systematic study and for future advanced research is performed giving effect to be considered desirable. | - |
dc.language | Korean | - |
dc.language.iso | ko | - |
dc.publisher | 대한치과기공학회 | - |
dc.title | 베릴륨이 포함되지 않은 도재용착주조관용 비 귀금속 합금의 재사용에 따른 금속과 도재간의 전단결합강도에 관한 연구 | - |
dc.title.alternative | The study of Shear Bond Strength on recasting of non-beryllium non-precious alloy for Porcelain between Metal | - |
dc.type | Article | - |
dc.contributor.affiliatedAuthor | 김웅철 | - |
dc.contributor.affiliatedAuthor | 김혜영 | - |
dc.contributor.affiliatedAuthor | 김지환 | - |
dc.identifier.bibliographicCitation | 대한치과기공학회지, v.35, no.1, pp.43 - 48 | - |
dc.relation.isPartOf | 대한치과기공학회지 | - |
dc.citation.title | 대한치과기공학회지 | - |
dc.citation.volume | 35 | - |
dc.citation.number | 1 | - |
dc.citation.startPage | 43 | - |
dc.citation.endPage | 48 | - |
dc.type.rims | ART | - |
dc.identifier.kciid | ART001753363 | - |
dc.description.journalClass | 2 | - |
dc.description.journalRegisteredClass | kci | - |
dc.description.journalRegisteredClass | other | - |
dc.subject.keywordAuthor | non-precious Alloy | - |
dc.subject.keywordAuthor | non-beryllium | - |
dc.subject.keywordAuthor | Recasting | - |
dc.subject.keywordAuthor | Shear Bond Strength | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
(02841) 서울특별시 성북구 안암로 14502-3290-1114
COPYRIGHT © 2021 Korea University. All Rights Reserved.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.