Effects of annealing atmosphere on the structural and electrical properties of (Na0.5K0.5)NbO3 thin films grown by RF magnetron sputtering
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Kim, Bo-Yun | - |
dc.contributor.author | Seong, Tae-Geun | - |
dc.contributor.author | Seo, In-Tae | - |
dc.contributor.author | Jang, Min-Soo | - |
dc.contributor.author | Nahm, Sahn | - |
dc.contributor.author | Kang, Jong-Yun | - |
dc.contributor.author | Yoon, Seok-Jin | - |
dc.date.accessioned | 2021-09-06T21:52:11Z | - |
dc.date.available | 2021-09-06T21:52:11Z | - |
dc.date.created | 2021-06-18 | - |
dc.date.issued | 2012-04 | - |
dc.identifier.issn | 1359-6454 | - |
dc.identifier.uri | https://scholar.korea.ac.kr/handle/2021.sw.korea/108869 | - |
dc.description.abstract | Amorphous (Na0.5K0.5)NbO3 (NKN) thin films were grown at 300 degrees C and subsequently annealed at 800 degrees C under Na2O, K2O and NKN atmospheres. When the annealing time was less than 50 min, K6Nb10.88O30 and Na2Nb4O11 secondary phases were formed in all the films. Moreover, they were also found in films annealed at 750 C for 180 min under NKN atmosphere, indicating that they were transient phases formed when the sintering time and temperature were not sufficient. For the film annealed for 50 min under Na2O atmosphere, an Na-excess (Na1-xKx)NbO3 (N1-xKxN) phase was formed, whereas a K-excess N1-xKxN phase was developed in the film annealed under K2O atmosphere. On the other hand, a homogeneous NKN phase was developed in the film annealed under NKN atmosphere and this was maintained after a long period (100 min) of annealing at 800 degrees C. A high leakage current density and a small dielectric constant (epsilon(r)) were observed for films annealed under Na2O and K2O atmospheres due to the evaporation of K2O and Na2O, respectively. Moreover, they exhibited a small remnant polarization (P-r) and a small coercive electric field (E-c). On the other hand, the film annealed under NKN atmosphere exhibited a very low leakage current density of 2.6 x 10(-9) A cm(-2) at 0.2 MV cm(-1) and had good ferroelectric and piezoelectric properties of epsilon(r) = 620, P-r = 11.7 mu C cm(-2), E-c = 133.8 kV cm(-1) and d(33) = 74 pm V-2 at 50 kV cm(-1). (C) 2012 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved. | - |
dc.language | English | - |
dc.language.iso | en | - |
dc.publisher | PERGAMON-ELSEVIER SCIENCE LTD | - |
dc.subject | FREE PIEZOELECTRIC CERAMICS | - |
dc.subject | MICROSTRUCTURE | - |
dc.subject | SUBSTRATE | - |
dc.subject | BEHAVIOR | - |
dc.title | Effects of annealing atmosphere on the structural and electrical properties of (Na0.5K0.5)NbO3 thin films grown by RF magnetron sputtering | - |
dc.type | Article | - |
dc.contributor.affiliatedAuthor | Nahm, Sahn | - |
dc.contributor.affiliatedAuthor | Kang, Jong-Yun | - |
dc.identifier.doi | 10.1016/j.actamat.2012.02.015 | - |
dc.identifier.scopusid | 2-s2.0-84862804843 | - |
dc.identifier.wosid | 000303952000059 | - |
dc.identifier.bibliographicCitation | ACTA MATERIALIA, v.60, no.6-7, pp.3107 - 3112 | - |
dc.relation.isPartOf | ACTA MATERIALIA | - |
dc.citation.title | ACTA MATERIALIA | - |
dc.citation.volume | 60 | - |
dc.citation.number | 6-7 | - |
dc.citation.startPage | 3107 | - |
dc.citation.endPage | 3112 | - |
dc.type.rims | ART | - |
dc.type.docType | Article | - |
dc.description.journalClass | 1 | - |
dc.description.journalRegisteredClass | scie | - |
dc.description.journalRegisteredClass | scopus | - |
dc.relation.journalResearchArea | Materials Science | - |
dc.relation.journalResearchArea | Metallurgy & Metallurgical Engineering | - |
dc.relation.journalWebOfScienceCategory | Materials Science, Multidisciplinary | - |
dc.relation.journalWebOfScienceCategory | Metallurgy & Metallurgical Engineering | - |
dc.subject.keywordPlus | FREE PIEZOELECTRIC CERAMICS | - |
dc.subject.keywordPlus | MICROSTRUCTURE | - |
dc.subject.keywordPlus | SUBSTRATE | - |
dc.subject.keywordPlus | BEHAVIOR | - |
dc.subject.keywordAuthor | Lead-free | - |
dc.subject.keywordAuthor | NKN thin film | - |
dc.subject.keywordAuthor | Piezoelectricity | - |
dc.subject.keywordAuthor | Sputtering | - |
dc.subject.keywordAuthor | Annealing | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
(02841) 서울특별시 성북구 안암로 14502-3290-1114
COPYRIGHT © 2021 Korea University. All Rights Reserved.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.