Anti-reflection and hydrophobic characteristics of M-PDMS based moth-eye nano-patterns on protection glass of photovoltaic systems
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Shin, Ju-Hyeon | - |
dc.contributor.author | Han, Kang-Soo | - |
dc.contributor.author | Lee, Heon | - |
dc.date.accessioned | 2021-09-07T13:02:25Z | - |
dc.date.available | 2021-09-07T13:02:25Z | - |
dc.date.created | 2021-06-14 | - |
dc.date.issued | 2011-05 | - |
dc.identifier.issn | 1062-7995 | - |
dc.identifier.uri | https://scholar.korea.ac.kr/handle/2021.sw.korea/112601 | - |
dc.description.abstract | To maximize the incident light, moth-eye nano-patterns were formed on a glass plate that was used as the protection glass for photovoltaic systems. These moth-eye nano-patterns were formed using a nano-imprint lithography process and increased the transmittance of the glass plate by minimizing the reflection of light at the surface. After the formation of the moth-eye nano-patterns, the surface was coated with a trichloro-silane based self-assembled monolayer in order to create a hydrophobic surface because the hydrophobic surface induced a self-cleaning effect. The transmittance of the glass plate increased from 91 to 94% at wavelength of 500 nm after the moth-eye structure was introduced. Thus, the short circuit current (J(SC)) of the I-V characteristics and the charged capacity of the photovoltaic system increased up to 6% after replacing the conventional protection glass with the moth-eye nano-patterned glass. The durability of the moth-eye nano-patterns was evaluated with respect to an acidic environment, high temperatures and UV irradiation. From these evaluation results, the values of the transmittance and contact angle did not decrease after the nano-patterns were soaked in sulfuric acid solutions with a pH of 2.0 for 48 h, exposed to a temperature of 120 degrees C for 48 h, and irradiated 10 times with UV light for 4 h. Copyright (C) 2010 John Wiley & Sons, Ltd. | - |
dc.language | English | - |
dc.language.iso | en | - |
dc.publisher | WILEY-BLACKWELL | - |
dc.subject | NANOIMPRINT LITHOGRAPHY | - |
dc.subject | FABRICATION | - |
dc.subject | DEPOSITION | - |
dc.subject | POLYMERS | - |
dc.subject | SURFACES | - |
dc.subject | IMPRINT | - |
dc.title | Anti-reflection and hydrophobic characteristics of M-PDMS based moth-eye nano-patterns on protection glass of photovoltaic systems | - |
dc.type | Article | - |
dc.contributor.affiliatedAuthor | Lee, Heon | - |
dc.identifier.doi | 10.1002/pip.1051 | - |
dc.identifier.scopusid | 2-s2.0-79953655402 | - |
dc.identifier.wosid | 000289518200013 | - |
dc.identifier.bibliographicCitation | PROGRESS IN PHOTOVOLTAICS, v.19, no.3, pp.339 - 344 | - |
dc.relation.isPartOf | PROGRESS IN PHOTOVOLTAICS | - |
dc.citation.title | PROGRESS IN PHOTOVOLTAICS | - |
dc.citation.volume | 19 | - |
dc.citation.number | 3 | - |
dc.citation.startPage | 339 | - |
dc.citation.endPage | 344 | - |
dc.type.rims | ART | - |
dc.type.docType | Article | - |
dc.description.journalClass | 1 | - |
dc.description.journalRegisteredClass | scie | - |
dc.description.journalRegisteredClass | scopus | - |
dc.relation.journalResearchArea | Energy & Fuels | - |
dc.relation.journalResearchArea | Materials Science | - |
dc.relation.journalResearchArea | Physics | - |
dc.relation.journalWebOfScienceCategory | Energy & Fuels | - |
dc.relation.journalWebOfScienceCategory | Materials Science, Multidisciplinary | - |
dc.relation.journalWebOfScienceCategory | Physics, Applied | - |
dc.subject.keywordPlus | NANOIMPRINT LITHOGRAPHY | - |
dc.subject.keywordPlus | FABRICATION | - |
dc.subject.keywordPlus | DEPOSITION | - |
dc.subject.keywordPlus | POLYMERS | - |
dc.subject.keywordPlus | SURFACES | - |
dc.subject.keywordPlus | IMPRINT | - |
dc.subject.keywordAuthor | moth-eye pattern | - |
dc.subject.keywordAuthor | M-PDMS | - |
dc.subject.keywordAuthor | nano-imprint lithography | - |
dc.subject.keywordAuthor | photovoltaic system | - |
dc.subject.keywordAuthor | transmittance, self-cleaning | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
145 Anam-ro, Seongbuk-gu, Seoul, 02841, Korea+82-2-3290-2963
COPYRIGHT © 2021 Korea University. All Rights Reserved.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.