Electrochemical behavior of a micro-patterned Si anode/LiV3O8 secondary cell
DC Field | Value | Language |
---|---|---|
dc.contributor.author | Jin, Dae-Gun | - |
dc.contributor.author | Yang, Ki-Yeon | - |
dc.contributor.author | Lee, Heon | - |
dc.contributor.author | Yoon, Woo Young | - |
dc.date.accessioned | 2021-09-07T22:22:06Z | - |
dc.date.available | 2021-09-07T22:22:06Z | - |
dc.date.created | 2021-06-14 | - |
dc.date.issued | 2010-12 | - |
dc.identifier.issn | 1388-2481 | - |
dc.identifier.uri | https://scholar.korea.ac.kr/handle/2021.sw.korea/115174 | - |
dc.description.abstract | Using a micro-patterned Si plate, a Li secondary cell was assembled and tested for its electrochemical properties. A micro-patterned Si plate was made by photolithography. This was followed by Pt coating and Li deposition. With a non-lithiated LiV3O8 cathode, a Li-deposited micro-patterned Si anode was assembled as a secondary cell. The cell exhibited an initial charge/discharge capacity of about 220 mAh g(-1) at a current density of 0.1 C-rate and it continued for more than 100 cycles without failure. The morphologies of Li deposition/dissolution in the anode were observed via scanning electron microscopy (SEM). Dendrite behavior of the Li metal was not observed on the anode during the cyclic process. (C) 2010 Elsevier B.V. All rights reserved. | - |
dc.language | English | - |
dc.language.iso | en | - |
dc.publisher | ELSEVIER SCIENCE INC | - |
dc.subject | OPTICAL-CELL | - |
dc.subject | LITHIUM | - |
dc.subject | ELECTRODE | - |
dc.subject | MORPHOLOGY | - |
dc.subject | SURFACE | - |
dc.subject | INTERFACES | - |
dc.subject | BATTERIES | - |
dc.title | Electrochemical behavior of a micro-patterned Si anode/LiV3O8 secondary cell | - |
dc.type | Article | - |
dc.contributor.affiliatedAuthor | Lee, Heon | - |
dc.contributor.affiliatedAuthor | Yoon, Woo Young | - |
dc.identifier.doi | 10.1016/j.elecom.2010.09.027 | - |
dc.identifier.scopusid | 2-s2.0-78649695275 | - |
dc.identifier.wosid | 000285904700007 | - |
dc.identifier.bibliographicCitation | ELECTROCHEMISTRY COMMUNICATIONS, v.12, no.12, pp.1694 - 1697 | - |
dc.relation.isPartOf | ELECTROCHEMISTRY COMMUNICATIONS | - |
dc.citation.title | ELECTROCHEMISTRY COMMUNICATIONS | - |
dc.citation.volume | 12 | - |
dc.citation.number | 12 | - |
dc.citation.startPage | 1694 | - |
dc.citation.endPage | 1697 | - |
dc.type.rims | ART | - |
dc.type.docType | Article | - |
dc.description.journalClass | 1 | - |
dc.description.journalRegisteredClass | scie | - |
dc.description.journalRegisteredClass | scopus | - |
dc.relation.journalResearchArea | Electrochemistry | - |
dc.relation.journalWebOfScienceCategory | Electrochemistry | - |
dc.subject.keywordPlus | OPTICAL-CELL | - |
dc.subject.keywordPlus | LITHIUM | - |
dc.subject.keywordPlus | ELECTRODE | - |
dc.subject.keywordPlus | MORPHOLOGY | - |
dc.subject.keywordPlus | SURFACE | - |
dc.subject.keywordPlus | INTERFACES | - |
dc.subject.keywordPlus | BATTERIES | - |
dc.subject.keywordAuthor | Micro-patterned Si anode | - |
dc.subject.keywordAuthor | Li metal | - |
dc.subject.keywordAuthor | Dendrite | - |
dc.subject.keywordAuthor | Secondary cell | - |
dc.subject.keywordAuthor | LiV3O8 | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
(02841) 서울특별시 성북구 안암로 14502-3290-1114
COPYRIGHT © 2021 Korea University. All Rights Reserved.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.