Continuous activation of Li2MnO3 component upon cycling in Li1.167Ni0.233Co0.100Mn0.467Mo0.033O2 cathode material for lithium ion batteries
DC Field | Value | Language |
---|---|---|
dc.contributor.author | 유승호 | - |
dc.date.accessioned | 2022-04-11T12:43:17Z | - |
dc.date.available | 2022-04-11T12:43:17Z | - |
dc.date.created | 2022-04-08 | - |
dc.date.issued | 2013-01 | - |
dc.identifier.issn | 2050-7488 | - |
dc.identifier.uri | https://scholar.korea.ac.kr/handle/2021.sw.korea/140017 | - |
dc.description.abstract | Li-rich layered cathode materials are very promising candidates for next generation high energy lithium ion batteries. One of the Li-rich layered cathode materials, Li1.167Ni0.233Co0.100Mn0.467Mo0.033O2 is prepared by a co-precipitation method. In this report, we focus on anomalous changes upon cycling in Li1.167Ni0.233Co0.100Mn0.467Mo0.033O2 cathode material in a voltage range of 2.0-4.55 V at room temperature. The structural transitions upon cycling are analyzed by ex situ X-ray diffraction. In addition, the changes in local structure during cycling are studied by X-ray absorption near edge structure. With differential capacity plots by controlling the cut-off voltage, the voltage decay during cycling is intensively studied. The continuous activation process of the residual Li2MnO3 component during cycling is correlated with voltage decay during cycling, and increasing capacity during the initial several cycles. Also, the electrochemical performance in Li1.167Ni0.233Co0.100Mn0.467Mo0.033O2 cathode material below 4.4 V is discussed. Furthermore, cycle performance is improved by reassembling Li1.167Ni0.233Co0.100Mn0.467Mo0.033O2 into another cell after washing. | - |
dc.language | English | - |
dc.language.iso | en | - |
dc.publisher | ROYAL SOC CHEMISTRY | - |
dc.title | Continuous activation of Li2MnO3 component upon cycling in Li1.167Ni0.233Co0.100Mn0.467Mo0.033O2 cathode material for lithium ion batteries | - |
dc.type | Article | - |
dc.contributor.affiliatedAuthor | 유승호 | - |
dc.identifier.doi | 10.1039/c2ta00309k | - |
dc.identifier.bibliographicCitation | JOURNAL OF MATERIALS CHEMISTRY A, v.1, pp.2833 - 2839 | - |
dc.relation.isPartOf | JOURNAL OF MATERIALS CHEMISTRY A | - |
dc.citation.title | JOURNAL OF MATERIALS CHEMISTRY A | - |
dc.citation.volume | 1 | - |
dc.citation.startPage | 2833 | - |
dc.citation.endPage | 2839 | - |
dc.type.rims | ART | - |
dc.type.docType | Article | - |
dc.description.journalClass | 1 | - |
dc.description.journalRegisteredClass | scie | - |
dc.description.journalRegisteredClass | scopus | - |
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.
(02841) 서울특별시 성북구 안암로 14502-3290-1114
COPYRIGHT © 2021 Korea University. All Rights Reserved.
Certain data included herein are derived from the © Web of Science of Clarivate Analytics. All rights reserved.
You may not copy or re-distribute this material in whole or in part without the prior written consent of Clarivate Analytics.