Recombination Zone Control without Sensing Layer and the Exciton Confinement in Green Phosphorescent OLEDs by Excluding Interface Energy Transfer

Authors
Jesuraj, P. JustinHafeez, HassanKim, Dong HyunLee, Jong ChanLee, Won HoChoi, Dae KeunKim, Chul HoonSong, MyungkwanKim, Chang SuRyu, Seung Yoon
Issue Date
8-2월-2018
Publisher
AMER CHEMICAL SOC
Citation
JOURNAL OF PHYSICAL CHEMISTRY C, v.122, no.5, pp.2951 - 2958
Indexed
SCIE
SCOPUS
Journal Title
JOURNAL OF PHYSICAL CHEMISTRY C
Volume
122
Number
5
Start Page
2951
End Page
2958
URI
https://scholar.korea.ac.kr/handle/2021.sw.korea/77368
DOI
10.1021/acs.jpcc.7b11039
ISSN
1932-7447
Abstract
We report the confinement of recombination zone (RZ) in green phosphorescent organic light-emitting diodes (Ph-OLEDs) for enhanced efficiency by varying the emission layer (EML) thickness and through quantum well (QW) insertion. At low thickness of EML, the efficiency is reduced owing to the diffusion of the RZ toward the EML/hole transport layer interface, which was revealed through the presence of exciton blocking layer [TCTA: tris(4-carbazoyl-9-ylphenyl)amine] excitation accompanied by a blue-shift in electroluminescence (EL). Further increase in the thickness of the EML caused the RZ to move toward the cathode, which was determined based on the disappearance Of TCTA emission and the corresponding red-shift observed in EL spectra. The solid-state and time-resolved area normalized photoluminescence emission spectra investigations further corroborate the RZ movement tactics along with TCTA excimer generation and exciplex generation between TCTA and tris[2-phenylpyridinato-C2,N]iridium(III) Ir(ppy)(3). The superior quantum and current efficiency of 14.4% and 50 cd/A, respectively, were determined for the device with an EML thickness of 15 nm due to the confinement of the RZ in the EML. The addition of (EML/interlayer/EML) QW facilitates improved charge balance in the Ph-OLED and further. assists in the confinement of the RZ in the EML. Because of QW, a slight increment in quantum (14.6%) and current efficiency (52 cd/A) was observed. Without using any sensing layers, movement of the RZ was successfully monitored and confined in the EML to realize enhanced efficiency in green Ph-OLEDs.
Files in This Item
There are no files associated with this item.
Appears in
Collections
Graduate School > Department of Advanced Materials Chemistry > 1. Journal Articles
Graduate School > Department of Applied Physics > 1. Journal Articles