High-performance amorphous donor-acceptor conjugated polymers containing x-shaped anthracene-based monomer and 2,5-bis(2-octyldodecyl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione for organic thin-film transistors
- Authors
- Lee, Joo Bin; Kim, Kyung Hwan; Hong, Chang Seop; Choi, Dong Hoon
- Issue Date
- 15-7월-2012
- Publisher
- WILEY
- Keywords
- charge transport; conjugated polymer; copolymerization; synthesis; heteroatom-containing polymers; noncrystalline polymers
- Citation
- JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY, v.50, no.14, pp.2809 - 2818
- Indexed
- SCIE
SCOPUS
- Journal Title
- JOURNAL OF POLYMER SCIENCE PART A-POLYMER CHEMISTRY
- Volume
- 50
- Number
- 14
- Start Page
- 2809
- End Page
- 2818
- URI
- https://scholar.korea.ac.kr/handle/2021.sw.korea/107929
- DOI
- 10.1002/pola.26078
- ISSN
- 0887-624X
- Abstract
- New diketopyrrolopyrrole (DPP)-containing amorphous conjugated polymers, such as poly(3-(5-((9,10-bis((4-hexylphenyl)ethynyl)-6-(prop-1-ynyl)anthracen-2-yl)ethynyl) thiophen-2-yl)-5-(2-hexyldecyl)-2-(2-octyldodecyl)-6-(thiophen-2-yl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione) (4), and poly(3-(5-((2,6-bis((4-hexylphenyl)ethynyl)-10-(prop-1-ynyl)anthracen-9-yl)ethynyl)thiophen-2-yl)-2,5-bis(2-octyldodecyl)-6-(thio phen-2-yl)pyrrolo[3,4-c]pyrrole-1,4(2H,5H)-dione) (7), were successfully synthesized via Sonogashira coupling reactions under microwave conditions. Copolymer 7, incorporating a DPP moiety at the 9,10-position of the anthracene ring through a triple bond, showed a much lower bandgap energy (Eg = 1.81 eV) than copolymer 4 (Eg = 2.13 eV). Tuning of the molecular frontier orbital energies was achieved by only changing the anchoring position of dithiophenyl-DPP from the 2,6- to the 9,10-position in the anthracene ring. Because of the donoracceptor (DA) interaction and the two-dimensional planar structure of the X-shaped donor monomer, the resulting polymers showed good interchain p-p stacking in the thin-film state, despite being amorphous polymers. When the newly synthesized polymer 7 was used as a semiconductor material in an organic thin-film transistor, the best mobility of up to 0.12 cm2 V-1 s-1 (Ion/off = similar to 4.4 x 10(6)) was observed, which is one of the highest values recorded for amorphous polymer films reported to date. (C) 2012 Wiley Periodicals, Inc. J Polym Sci Part A: Polym Chem, 2012
- Files in This Item
- There are no files associated with this item.
- Appears in
Collections - College of Science > Department of Chemistry > 1. Journal Articles
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.