Fine size (Y,Gd)BO3:Eu phosphor powders prepared from precursor powders with hollow shape and large size
- Authors
- Koo, Hye Young; Ko, Da Rae; Lee, Sang Ho; Lee, Su Min; Kang, Yun Chan; Lee, Jong-Heun
- Issue Date
- 30-7월-2010
- Publisher
- ELSEVIER SCIENCE SA
- Keywords
- Chemical synthesis; Gas-solid reaction
- Citation
- JOURNAL OF ALLOYS AND COMPOUNDS, v.503, no.1, pp.260 - 265
- Indexed
- SCIE
SCOPUS
- Journal Title
- JOURNAL OF ALLOYS AND COMPOUNDS
- Volume
- 503
- Number
- 1
- Start Page
- 260
- End Page
- 265
- URI
- https://scholar.korea.ac.kr/handle/2021.sw.korea/116036
- DOI
- 10.1016/j.jallcom.2010.05.012
- ISSN
- 0925-8388
- Abstract
- Fine size (Y,Gd)BO3:Eu phosphor powders with high photoluminescence intensity under vacuum ultraviolet were prepared by spray pyrolysis. The precursor powders with hollow shape and large size were prepared by spray pyrolysis from the spray solution with citric acid. The precursor powders turned to the (Y,Gd)BO3:Eu phosphor powders after post-treatment at temperatures between 900 and 1100 degrees C. The mean sizes of the phosphor powders post-treated at a temperature of 950 degrees C were 0.37 mu m. The photoluminescence intensity of the fine size (Y,Gd)BO3:Eu phosphor powders was 95% of that of the commercial (Y,Gd)BO3:Eu phosphor powders with micron sizes. (C) 2010 Elsevier B.V. All rights reserved.
- Files in This Item
- There are no files associated with this item.
- Appears in
Collections - College of Engineering > Department of Materials Science and Engineering > 1. Journal Articles
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.