High response and selectivity toward hydrogen gas detection by In2O3 doped Pd@ZnO core-shell nanoparticles
- Authors
- Nguyen, Thuy T. D.; Dung Van Dao; Lee, In-Hwan; Yu, Yeon-Tae; Oh, Sang-Yeob
- Issue Date
- 15-2월-2021
- Publisher
- ELSEVIER SCIENCE SA
- Keywords
- Palladium; Zinc oxide; Core-shell; Hydrogen gas sensing
- Citation
- JOURNAL OF ALLOYS AND COMPOUNDS, v.854
- Indexed
- SCIE
SCOPUS
- Journal Title
- JOURNAL OF ALLOYS AND COMPOUNDS
- Volume
- 854
- URI
- https://scholar.korea.ac.kr/handle/2021.sw.korea/49566
- DOI
- 10.1016/j.jallcom.2020.157280
- ISSN
- 0925-8388
- Abstract
- An efficient hydrogen gas sensor comprising 5 wt% In2O3 doped in Pd@ZnO core-shell nanoparticles (Pd@ZnO-In2O3 CSNPs) was synthesized via a facile hydrothermal approach. The obtained material has a higher Brunauer-Emmett-Teller surface area (80 m(2) g(-1)) compared to Pd@ZnO (56 m(2) g(-1)) and pure ZnO (40 m(2) g(-1)). The Pd@ZnO-In2O3 sensor achieved the maximal response (42) to 100 ppm hydrogen at 300 degrees C. Whereas, Pd@ZnO and pure ZnO sensors exhibited lower responses (17 and 9) to 100 ppm hydrogen at a higher optimal temperature (350 degrees C). It also demonstrated faster response and recovery time (0.4 and 4.0 min) than those obtained from Pd@ZnO (1.4 and 14 min) and pure ZnO (6.0 and 18.0 min) sensors. The hydrogen sensing enhancement of Pd@ZnO-In2O3 materials could be largely attributed to the synergistic electronic and chemical activities of Pd, ZnO and In2O3 parts, and its large surface area. Especially, due to the ability to adsorb hydrogen of the core, Pd based sensors exhibited high selectivity to hydrogen with respect to Pd-free sensors. (C) 2020 Elsevier B.V. All rights reserved.
- Files in This Item
- There are no files associated with this item.
- Appears in
Collections - College of Engineering > Department of Materials Science and Engineering > 1. Journal Articles
Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.