Detailed Information

Cited 0 time in webofscience Cited 0 time in scopus
Metadata Downloads

Effect of the amine group content on catalytic activity and stability of mesoporous silica supported Pd catalysts for additive-free formic acid dehydrogenation at room temperature

Authors
Jin, Min-HoPark, Ju-HyoungOh, DuckkyuPark, Jong-SooLee, Kwan-YoungLee, Dong-Wook
Issue Date
22-2월-2019
Publisher
PERGAMON-ELSEVIER SCIENCE LTD
Citation
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, v.44, no.10, pp.4737 - 4744
Indexed
SCIE
SCOPUS
Journal Title
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY
Volume
44
Number
10
Start Page
4737
End Page
4744
URI
https://scholar.korea.ac.kr/handle/2021.sw.korea/67592
DOI
10.1016/j.ijhydene.2018.12.208
ISSN
0360-3199
Abstract
A strong metal-support interaction (SMSI) between amine-functionalized silica supports and Pd nanoparticles is one of important factors to determine the catalytic activity of additive-free formic acid dehydrogenation at room temperature over Pd/NH2-silica catalysts. However, there are few reports on the effect of the content of amine functional groups on the SMSI and catalytic performance for formic acid dehydrogenation. In this study, we tried to maximize the content of amino-propyl groups on the surface of mesoporous silica supports (KIE-6) via hydroxylation of KIE-6 surface before amine functionalization and investigated the effect of the content of amine functional groups on the catalytic activity and stability for formic acid dehydrogenation. As a result, Pd/NH2-hydroxylated KIE-6 (Pd/NH2-OH-KIE-6) catalysts with more amine functional groups provided higher initial catalytic activity (595 mol H-2 mol catalyst(-1)h(-1)) than Pd/NH2-KIE-6 catalysts. However, Pd/NH2-KIE-6 catalysts showed higher catalytic stability in comparison with Pd/NH2-OH-KIE-6 catalysts. After various characterizations of catalysts, it was demonstrated that the enhanced initial catalytic activity of Pd/NH2-OH-KIE-6 catalysts is attributed to the higher ratio of Pd/PdO derived from the increased content of amine groups of NH2-OH-KIE-6 supports. In contrast, the low surface area of NH2-OH-KIE-6 promoted the aggregation of Pd nanoparticles on Pd/NH2-OH-KIE-6 catalysts, which resulted in the lower catalytic stability of Pd/NH2-OH-KIE-6 catalysts than Pd/NH2-KIE-6 catalysts. Thus it was concluded that confinement of Pd nanoparticles to the pores of supports is a more dominant factor to achieve higher catalytic stability, while the initial catalytic activity is affected by the electronic state of Pd nanoparticle determined by the content of amine functional groups on the surface of supports. (C) 2019 Hydrogen Energy Publications LLC. Published by Elsevier Ltd. All rights reserved.
Files in This Item
There are no files associated with this item.
Appears in
Collections
College of Engineering > Department of Chemical and Biological Engineering > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Lee, Kwan Young photo

Lee, Kwan Young
공과대학 (화공생명공학과)
Read more

Altmetrics

Total Views & Downloads

BROWSE