Detailed Information

Cited 0 time in webofscience Cited 0 time in scopus
Metadata Downloads

Dielectric properties of single crystal Sr2Nb3O10 dielectric nanosheet thin films by electrophoretic deposition (EPD) and post deposition treatments

Authors
Lee, Young-ShinYim, HaenaYoo, So-YeonJu, Byeong-KwonChoi, Ji-Won
Issue Date
15-7월-2017
Publisher
ELSEVIER SCIENCE SA
Keywords
Nanosheet; Electrophoretic deposition; Post treatment; Dielectric properties
Citation
JOURNAL OF ALLOYS AND COMPOUNDS, v.711, pp.51 - 57
Indexed
SCIE
SCOPUS
Journal Title
JOURNAL OF ALLOYS AND COMPOUNDS
Volume
711
Start Page
51
End Page
57
URI
https://scholar.korea.ac.kr/handle/2021.sw.korea/82821
DOI
10.1016/j.jallcom.2017.03.342
ISSN
0925-8388
Abstract
Sr2Nb3O10 (SNO) nanosheets were obtained by exfoliating from a perovskite layered structure of HSr2Nb3O10 (HSNO). The nanosheets were deposited on substrates simultaneously with unintended tetrabutylammonium cations (TBA(+)) by electrophoretic deposition (EPD) process. To eliminate TBA+ from the SNO dielectric nanosheet thin films, the films were exposed to ultraviolet (UV). Since UV exposure can't decompose TBA(+) completely, thermal annealing was additionally conducted by employing different furnaces at various atmospheres. XRD shows the reduction in lattice constant after UV and thermal treatments, indicating that TBA cations were decomposed in the interlayer of nano sheets. FT-IR spectra analysis depicted that the organic materials were eliminated through the post deposition treatments. In addition, XPS data indicated that films treated by a combination of UV and thermal had a lower relative atomic ratio of carbon and nitrogen than as-deposited and only-UV treated films. The optimum process conditions for improving dielectric properties were UV exposure for 15 h and subsequent thermal annealing in a box furnace in the air at 600 degrees C for 1 h. When compared to the as deposited film, the dielectric constants of films further annealed by the box furnace in the air were increased from 8 to 27 at 1 MHz whereas dielectric loss (tan 8) decreased from 5% to 2%. Additional thermal treatment strongly affects nanosheets to decompose TBA(+). (C) 2017 Elsevier B.V. All rights reserved.
Files in This Item
There are no files associated with this item.
Appears in
Collections
College of Engineering > School of Electrical Engineering > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Ju, Byeong kwon photo

Ju, Byeong kwon
공과대학 (전기전자공학부)
Read more

Altmetrics

Total Views & Downloads

BROWSE