Effect of light-curing, pressure, oxygen inhibition, and heat on shear bond strength between bis-acryl provisional restoration and bis-acryl repair materials

Authors
Shim, Ji-SukLee, Jeong-YolChoi, Yeon-JoShin, Sang-WanRyu, Jae-Jun
Issue Date
Feb-2015
Publisher
KOREAN ACAD PROSTHODONTICS
Keywords
Bis-acryl; Repair; Relining; Heat; Shear bond strength
Citation
JOURNAL OF ADVANCED PROSTHODONTICS, v.7, no.1, pp.47 - 50
Indexed
SCIE
SCOPUS
KCI
Journal Title
JOURNAL OF ADVANCED PROSTHODONTICS
Volume
7
Number
1
Start Page
47
End Page
50
URI
https://scholar.korea.ac.kr/handle/2021.sw.korea/94499
DOI
10.4047/jap.2015.7.1.47
ISSN
2005-7806
Abstract
PURPOSE. This study aimed to discover a way to increase the bond strength between bis-acryl resins, using a comparison of the shear bond strengths attained from bis-acryl resins treated with light curing, pressure, oxygen inhibition, and heat. MATERIALS AND METHODS. Self-cured bis-acryl resin was used as both a base material and as a repair material. Seventy specimens were distributed into seven groups according to treatment methods: pressure - stored in a pressure cooker at 0.2 Mpa; oxygen inhibition- applied an oxygen inhibitor around the repaired material,; heat treatment - performed heat treatment in a dry oven at 60 degrees C, 100 C, or 140 degrees C. The shear bond strength was measured with a universal testing machine, and the shear bond strength (MPa) was calculated from the peak load of failure. A comparison of the bond strength between the repaired specimens was Conducted using one-way ANOVA and Tukey multiple comparison tests (alpha=.05). RESULTS. There were no statistically significant differences in the shear bond strength between the control group and the light curing, pressure, and oxygen inhibition groups. However, the heat treatment groups showed statistically higher bond strengths than the groups treated without heat, and the groups treated at a higher temperature resulted in higher bond strengths. Statistically significant differences were seen between groups after different degrees of heat treatment, except in groups heated at 100 C and 140 C. CONCLUSION. Strong bonding can be achieved between a bis-acryl base and bis-acryl repair material after heat treatment.
Files in This Item
There are no files associated with this item.
Appears in
Collections
College of Medicine > Department of Medical Science > 1. Journal Articles

qrcode

Items in ScholarWorks are protected by copyright, with all rights reserved, unless otherwise indicated.

Related Researcher

Researcher Ryu, Jae Jun photo

Ryu, Jae Jun
College of Medicine (Department of Medical Science)
Read more

Altmetrics

Total Views & Downloads

BROWSE